Choose the manufacturing route based on geometry, material, quantity and validation requirements.
Precision metal and engineering plastic parts from prototype through repeat production.
Tooling development, molded parts and production support for repeat plastic manufacturing.
Functional prototypes, complex geometry and low-volume parts without conventional tooling.
Explore 3D PrintingStart with geometry, material, quantity and critical requirements before selecting the route.
Request Engineering ReviewReview manufacturability, tolerances, inspection strategy and production readiness.
Design, materials and manufacturing resources for better process decisions before production.
Real manufacturing, tooling and validation decisions applied under project conditions.
Manufacturing support aligned with functional, quality and validation requirements.
Manufacturing facilities, quality systems and engineering support behind SPI.
Send your CAD, drawing, material and quantity for an initial manufacturing review.
Request Engineering ReviewType II, Type III & Tolerances
Anodizing changes more than an aluminum part’s color. Its oxide layer can affect fit, edge conditions, thread engagement, and the appearance of machined surfaces. For CNC parts, the specification must balance corrosion resistance, wear needs, cosmetic expectations, and critical dimensions.
Type II is commonly used for protective and decorative finishes; Type III is considered when greater surface hardness and wear resistance are needed. The choice also depends on alloy, pretreatment, coating thickness, masking, and final drawing dimensions.
This guide explains how to specify the finish, flag features that may need masking, and agree on sample approval and inspection before production. For broader process comparisons, see our CNC surface finishing guide ; for machining and quotes, visit CNC machining services .
Process Selection
Choose an anodizing type according to the part's functional requirements, not appearance alone. Type II is commonly used for protective and decorative finishes; Type III is considered when greater surface hardness and wear resistance are required.
| Decision factor | Type II — Sulfuric Anodizing | Type III — Hardcoat Anodizing |
|---|---|---|
| Primary purpose | General corrosion protection and decorative finishes. | Applications requiring a harder, more wear-resistant oxide layer. |
| Wear requirements | Suitable when ordinary protective performance meets the specification. | Consider for sliding contact, abrasion or demanding wear conditions. |
| Appearance | Often offers more flexibility for decorative colors, depending on alloy and process. | May produce darker or less uniform-looking finishes, depending on alloy, thickness and processing. |
| Dimensions and fit | Coating growth can affect holes, threads and mating features. | Greater coating build may create additional dimensional constraints. |
| Best starting point | Define appearance, corrosion exposure and required protection. | Define wear conditions, coating requirements and critical dimensions. |
Engineering rule: Specify the anodizing type, applicable standard, required coating thickness and acceptance criteria on the drawing. Confirm masking and final dimensions before production. Neither type guarantees a particular color or fit without process-specific review.
Actual coating performance and dimensional effects depend on alloy, temper, geometry, pretreatment and process conditions. Confirm requirements with the selected anodizing supplier against the applicable specification.
Dimensional Control
Anodizing changes surface dimensions. Final fit depends on alloy, coating specification, part geometry, and process control—not a universal allowance.
For close-tolerance CNC parts, review bores, reamed holes, threads, slots, mating faces, and datum features before release. Coating growth can reduce clearance or affect thread engagement, while edges and deep recesses may finish differently from open surfaces.
Mark non-coated areas and electrical contact points clearly on the drawing. Identify whether masking is required for precision bores, threads, bearing seats, grounding points, or sealing faces. Confirm with the anodizing supplier which surfaces can be masked consistently.
State whether critical dimensions apply before or after anodizing, and define the inspection condition. Where fit is sensitive, agree on a representative sample or first-article check before production.
Engineering rule: Do not apply a blanket machining allowance to every feature. Review critical fits against the specified coating process and verify the finished part against the drawing.
Appearance & Quality Verification
Anodized appearance depends on alloy chemistry, temper, surface preparation, coating process, and dye treatment. The alloy name alone cannot guarantee an exact shade or consistent matching between production lots.
For 6061, 7075, and 5052 parts, assess the finish against the actual material and application. Composition and machining or blasting can change brightness, color response, and visible texture. Do not assume different alloys will match under the same process. See our 6061 temper guide , 7075 aluminum machining guide , and 5052 alloy guide for material-specific context.
Define the cosmetic standard before production. Provide an approved sample, identify visible faces, and specify acceptable variation and viewing conditions. Confirm whether surfaces will be machined, brushed, or blasted, because preparation affects the final appearance.
For critical parts, approve a representative first article before batch release. Inspect appearance under agreed conditions and verify CTQ dimensions after finishing when required. Keep grade and temper traceable to the material certificate; record inspection results against the drawing revision.
Release rule: Confirm acceptance criteria on representative parts made with the agreed alloy and process. Do not rely on a color name alone to guarantee appearance consistency.
Drawing Release & RFQ
A useful anodizing RFQ turns appearance and performance expectations into measurable requirements. Avoid specifying only a color name: alloy, pretreatment, anodizing type, and acceptance conditions all influence the finished result.
If requirements are undecided, identify the operating environment and wear or corrosion exposure so the supplier can flag missing information before quotation. Confirm that the selected process meets the drawing and appearance standard before release.
Share your drawing, quantity, alloy, finish specification, and critical features through our CNC machining services inquiry path.
For inspection and documentation expectations, see our manufacturing quality documents guide .